VINYL / SCRIM / METALLIZED POLYESTER
FACING COMPOSITION DESCRIPTION VALUES (ENGLISH) VALUES (METRIC)
White Film Rigid Vinyl 0.0025 inch 63.5 micron
Adhesive Flame Resistant    
Reinforcing Bi-directional
Fiberglass
4 / inch (XD)
4 / inch (MD)
16 / 100 mm (MD)
16 100 mm (XD)
Film Metallized Polyester 0.0005 inch 12.7 micron
PHYSICAL PROPERTIES TEST METHOD VALUES (ENGLISH) VALUES (METRIC)
Basis Weight Scale 35 lbs / 1000 ft² 171 gm / m²
Permeance (WVTR) ASTM E96
Procedure A
0.02 perm(grains/hr.ft².in Hg) 1.15 ng / N.s
Bursting Strength ASTM D774 85 psi 6.0 kg / cm²
Puncture Resistance ASTM C1136 150 beach units 4.5 Joules
Tensile Strength ASTM C1136 40 lbs/inch width (MD)
30 lbs/inch width (XD)
7.0 kn / m (MD)
5.3 kn / m (XD)
Caliper / Thickness Micrometer 0.0010 inch 254 micron
Accelerated Aging 30 Days @95% RH, 120°F (49°C) No Corrosion
No Delamination
No Corrosion
No Delamination
Low Temperature Resistance ASTM D1790 10°F (-12°C) Remains Flexible
No Delamination
Remains Flexible
No Delamination
High Temperature Resistance 4 hours @150°F (66°C) Remains Flexible
No Delamination
Remains Flexible
No Delamination
Water Immersion 24 hours @ 73°F (23°C) No Delamination No Delamination
Mold Resistance ASTM C665 / C1338 No Growth No Growth
Dimensional Stability ASTM D1204 0.25% 0.25%
Light Reflectance ASTM C523 88.5% 88.5%
FIRE TESTING UL 723 / ASTM E84
Flame Spread Smoke Developed
Foil Exposed 15 50
Fabric Exposed 15 40

Physical Properties based upon statistical averages, Weight / Thickness +/- 10%


Setting the Standard Steel Building Benefits Benefits of DIY Why Choose Us Financing
Policy & Procedures
Customer Support
About Us Builder Information Employment Opportunities Photo Gallery Site Map

        We Gladly Accept Visa, Mastercard and Discover


Copyright © 2003-2024 MetalBuildingDepot™. All Rights Reserved. Privacy Policy